Welcome to our websites!

Factory Free sample New Type Silicon Calcium Metal as Deoxidizer for Iron Casting and Steelmaking

Performance and use

1. It contains 75% manganese and the rest is aluminum powder.

2. Environmental protection and pollution-free; the actual yield is greater than 95%.

3. It has obvious refining effect on the alloy.

4. It is suitable for the addition of manganese element and the refinement of grain structure in aluminum and other alloys.

 

Featured:

250g/bolck, 1kg/bag, 20kg/box

 

 


Product Detail

Product Tags

Our firm aims to operating faithfully, serving to all of our consumers , and working in new technology and new machine continually for Factory Free sample New Type Silicon Calcium Metal as Deoxidizer for Iron Casting and Steelmaking, We sincerely assume exchange and cooperation along with you. Let’s move forward hand in hand and achieve win-win problem.
Our firm aims to operating faithfully, serving to all of our consumers , and working in new technology and new machine continually for China Deoxidizer and Silicon Calcium Metal, We critically promise that we deliver all the customers with the best quality solutions, the most competitive prices and the most prompt delivery. We hope to win a resplendent future for customers and ourselves.
2. Use matters:

2.1 Adding temperature: >730°C.

2.2 The reference dosage of this product is calculated according to the following formula:

Mn   Mn tds

 

Note: Due to the difference between the user and the metallurgical conditions in the furnace, the actual yield and the actual addition amount should be calculated and determined based on the test data before the furnace.

2.3 Adding method:

After melting in the furnace, stir it evenly, take a sample and analyze it to calculate the amount of manganese agent added. When the melting temperature is reached, remove the dross on the surface of the melt, and disperse the product into various parts of the molten pool (if iron and copper agents need to be added, they can be added at the same time). After the reaction is complete, stand still for 5 minutes; fully stir, then stand still again for 20-30 minutes; melt completely, take samples for analysis, and then transfer to the next process if the ingredients are qualified.

 

3. Packaging and storage

20kg-25kg/box, plastic film or aluminum foil packaging, strictly prevent moisture, because the metal powder contained in the additive is highly active and easy to oxidize, and the flux contained in it is easy to be damp, the surface of the additive is oxidized after being wet, and in severe cases, there will be pulverization, which will affect the actual yield,or even invalidated.

 

4. Shelf life

Eight months, can use it directly after opening the box.

 Our firm aims to operating faithfully, serving to all of our consumers , and working in new technology and new machine continually for Factory Free sample New Type Silicon Calcium Metal as Deoxidizer for Iron Casting and Steelmaking, We sincerely assume exchange and cooperation along with you. Let’s move forward hand in hand and achieve win-win problem.