We have a minimum capacity of 500KG medium frequency furnace, electric furnace, etc. for aluminum plants with small output, and there are also fixed large-scale aluminum melting roads with a capacity of 5UST to 88UST, for aluminum casting plants with larger output. Aluminum Extrusion Aging Furnace, Cutting Aluminum Extrusion, Hot Top Billet Casting Machine, Refractory materials needed: heat storage balls, castables, refractory bricks, aluminum silicate cotton plates, plug heads, launder structures, ceramic foam filter plates, filter boxes, manifold plates, conduits, adapter plates, graphite rings, crystallizers.
Discount wholesale Slag Removing Flux - Liquid and solid Low Temperature Polishing Additive including oil degreasing – ZheLu Detail:

1.To determine the concentration of FL-01 and keep it within the range of operating condition,replenish in time.

2.It is better that the aluminum profiles should be rinsing once before the brightening process for avoiding too much aluminum debris and impurities be taken in, which will influence, degreasing effect and increase the consumption of Low Temperature Polishing Additive.

3.The bath should be cleaned regularly during production because there were some insoluble substances like mechanical sundries and dust.

Low Temperature Polishing Additive is packed with sealed plastic barrel, 30kg net each.

Low temperature polishing sink–assay method
Required reagents: 1N NaOH standard solution ②1% phenolphthalein indicator ③ Potassium

①Accurately pipette 20mL of the bath solution into a 250mL conical flask, add 50mL of distilled water, then add 2 to 3 drops of 1% phenolphthalein indicator, and titrate with 1N NaOH until the solution changes from colorless to pink, which is the end point. Write down V1 without fading within 30s.

②Accurately pipette 5mL of the sink solution into a 250mL conical flask, add 50mL of distilled water, add 3g of potassium fluoride, dissolve and shake well, add 2 to 3 drops of 1% phenolphthalein indicator, and titrate with 1N NaOH until the solution is Colorless to pink is the end point, and V2 is recorded if the color does not fade within 30s .

calculate
work point (number of points) = 9.8 × V 1 × N
Free acid ((g/L)=9.8×V 2 ×N

work point

free acid

temperature

90~130

20~35g/L

18~25℃


Product detail pictures:

Discount wholesale Slag Removing Flux - Liquid and solid Low Temperature Polishing Additive including oil degreasing – ZheLu detail pictures


Related Product Guide:

Foshan Zhelu not only provides sales services, but also helps companies in aluminum industry to solve all the problems. Welcome enquiries. Discount wholesale Slag Removing Flux - Liquid and solid Low Temperature Polishing Additive including oil degreasing – ZheLu , The product will supply to all over the world, such as: Tanzania, Muscat, Mongolia, Foshan Zhelu has successfully developed 6 series aluminum alloy profile products with high strength and high corrosion resistance, which can be used in ships and other fields.
  • A nice supplier in this industry, after a detail and careful discussion, we reached a consensus agreement. Hope that we cooperate smoothly.
    5 Stars By Fanny from Russia - 2018.07.27 12:26
    This is a very professional and honest Chinese supplier, from now on we fell in love with the Chinese manufacturing.
    5 Stars By Tom from Mauritania - 2017.04.08 14:55